求翻译:当钢的碳当量CE>0.6%时,淬硬倾向严重,焊接性差,焊接时需要较高的预热温度和采取严格的工艺措施。是什么意思?

待解决 悬赏分:1 - 离问题结束还有
当钢的碳当量CE>0.6%时,淬硬倾向严重,焊接性差,焊接时需要较高的预热温度和采取严格的工艺措施。
问题补充:

  • 匿名
2013-05-23 12:21:38
When the carbon equivalent of the steel ce> 0.6%, severe hardening tendency, poor welding, welding requires higher preheating temperature and to take strict measures of the process.
  • 匿名
2013-05-23 12:23:18
When the carbon steel CE > 0.6 % yield when serious tendency, hardened, welding, soldering, heat to a higher temperature and the adoption of strict process measures.
  • 匿名
2013-05-23 12:24:58
When steel carbon equivalent CE>0.6%, the hard tendency is serious, the weldability is bad, when welding needs the high preheating temperature and takes the strict craft measure.
  • 匿名
2013-05-23 12:26:38
When steel is carbon equivalent CE>0.6%, hardened tend to seriously, poor welding, weld preheat temperature and to higher when taking strict measures.
  • 匿名
2013-05-23 12:28:18
正在翻译,请等待...
 
 