求翻译:PURPOSE: A thin film-type cement terrazzo composition using a cement grout material of high strength is provided, which has excellent abrasion strength and flame resistance, generates no cracking and can be produced into the shape of a thin film. CONSTITUTION: The thin film-type cement terrazzo composition comprises ab是什么意思?

待解决 悬赏分:1 - 离问题结束还有
PURPOSE: A thin film-type cement terrazzo composition using a cement grout material of high strength is provided, which has excellent abrasion strength and flame resistance, generates no cracking and can be produced into the shape of a thin film. CONSTITUTION: The thin film-type cement terrazzo composition comprises ab
问题补充:

  • 匿名
2013-05-23 12:21:38
目的:使用高强度的水泥灌浆材料的薄膜型水泥水磨石组合物被提供,其具有优异的耐磨损强度和阻燃性,不产生裂纹,并且可以制作成薄膜状。
  • 匿名
2013-05-23 12:23:18
目的:高强度提供使用水泥水泥材料的稀薄的薄膜式水泥磨石子地构成,有优秀磨蚀力量和火焰抵抗,不引起崩裂并且可以被生产入薄膜的形状。
  • 匿名
2013-05-23 12:24:58
目的: 使用水泥水泥材料高强度没有提供稀薄的film-type水泥磨石子地构成,有优秀磨蚀力量和火焰抵抗,引起崩裂并且可以被生产入形状薄膜。 宪法: 稀薄的film-type水泥磨石子地构成包括大约35-55份按共同的波特兰水泥重量计算; 大约0.5-3.0份按萘重量计算磺酸盐根据superplasticizer为减少相当数量水; 大约3-8分开按硅土发烟重量计算为改进力量; 大约5-15分开按水泥泡胀剂重量计算为防止裂化和变形; 并且45-70份按基于白云岩的材料重量计算。
  • 匿名
2013-05-23 12:26:38
目的: 使用高强度水泥灌浆材料的薄胶片类型水泥水磨石组成是提供具有优异的耐磨强度和火焰抵抗,生成无开裂和可以制作成一层薄膜的形状。宪法 》: 薄胶片类型水泥水磨石成分约占 35-55 零件按重量的普通硅酸盐水泥 ;部分由萘磺酸盐减水剂为减少的水量 ; 重量约为 0.5-3.0约 3-8 部分重量由二氧化硅的油烟提高强度 ;大约 5-15 零件重量的油井水泥膨胀剂,防止开裂和变形 ;和基于白云石材料按重量 45-70 部分。