求翻译:Samples were prepared through a high energy ball milling process. Manganese powder (_325 mesh, 99.3%) and solid gallium (99.999%) were loaded into a tungsten carbidemixing vial with a nominal chemistry of Mn1_xGax with x¼0.20 by atomic mass. The vial was filled with argon andmilled for intermediate periods for a total 是什么意思? 待解决
悬赏分:1
- 离问题结束还有
Samples were prepared through a high energy ball milling process. Manganese powder (_325 mesh, 99.3%) and solid gallium (99.999%) were loaded into a tungsten carbidemixing vial with a nominal chemistry of Mn1_xGax with x¼0.20 by atomic mass. The vial was filled with argon andmilled for intermediate periods for a total
问题补充: |
|
2013-05-23 12:21:38
样品通过高能球磨方法制备的。
|
|
2013-05-23 12:23:18
样品通过一个高能球碾碎的过程准备了。锰粉末(_325滤网, 99.3%)和坚实镓(99.999%)被装载了入钨carbidemixing的小瓶用Mn1_xGax有名无实的化学用x ¼ 0.20由原子质量。小瓶充满了在中间期间andmilled的氩一个总时间的3 h在包含不锈钢球的一个高能磨房(SPEX 8000M)。
|
|
2013-05-23 12:24:58
样品通过一个高能球碾碎的过程准备了。 锰粉末 (_325滤网, 99.3%) 和坚实镓 (99.999%) 被装载了入钨carbidemixing的小瓶用Mn1_xGax有名无实的化学用x ¼ 0.20由原子质量。 小瓶充满了氩andmilled在中间期间一个总时间的3 h在高能磨房 (SPEX 8000M) 包含的不锈钢的球。 为2在搬空的石英管和热被按了,密封对待的被碾碎的粉末h在范围从280 _C的温度到350 _C。
|
|
2013-05-23 12:26:38
通过高能球磨工艺制备了样品。锰粉 (_325 目,99.3%) 和固态镓 (99.999%) 都被加载到 Mn1_xGax 与 x¼0.20 名义化学钨 carbidemixing 小瓶由原子质量。小瓶充满了氩 andmilled 中间一段的总时间为 3 h 在高能磨 (SPEX 8000 米) 含不锈钢钢球。磨碎的粉末被按下,密封在真空的石英管和热处理温度下从 280 _C 到 350 _C 2 h。
|
|
2013-05-23 12:28:18
正在翻译,请等待...
|
湖北省互联网违法和不良信息举报平台 | 网上有害信息举报专区 | 电信诈骗举报专区 | 涉历史虚无主义有害信息举报专区 | 涉企侵权举报专区