求翻译:We tested the stainless steel tubes for chemical composition, on the intergranular corrosion, mechanical testing. Unfortunately, the absence of titanium in the steel leads to intergranular corrosion, and to tendency to overheat steel. During the flaring of such pipes is not enough toughness of steel, it does not allow 是什么意思?

待解决 悬赏分:1 - 离问题结束还有
We tested the stainless steel tubes for chemical composition, on the intergranular corrosion, mechanical testing. Unfortunately, the absence of titanium in the steel leads to intergranular corrosion, and to tendency to overheat steel. During the flaring of such pipes is not enough toughness of steel, it does not allow
问题补充:

  • 匿名
2013-05-23 12:21:38
我们测试了不锈钢管的化学成分,对晶间腐蚀,机械测试。
  • 匿名
2013-05-23 12:23:18
我们为化学成分测试了不锈钢管,在晶间腐蚀,机械测试。不幸地,缺乏在钢的钛导致晶间腐蚀和倾向过度加热钢。在飘动的这样管子期间不是钢,它的足够的韧性不准许紧紧做飘动管子在tubesheet。当压力适用于设备时可能导致化合物的降压。
  • 匿名
2013-05-23 12:24:58
我们为化学成分测试了不锈钢的管,在晶间腐蚀,机械测试。 不幸地,缺乏钛在钢导致晶间腐蚀和倾向过度加热钢。 在飘动的这样管子期间不是钢,它的足够的韧性不准许紧紧做飘动管子在tubesheet。 当压力适用于设备时可以导致化合物的降压。
  • 匿名
2013-05-23 12:26:38
我们测试了不锈钢管的化学成分,对晶间腐蚀、 力学性能测试。不幸的是,在钢中钛的缺席导致晶间腐蚀和热钢的倾向。在这种管道的燃烧过程中不是足够的钢的韧性,它不允许,使燃烧管紧紧的管板。当施加压力,该设备可能会导致降压法的化合物。
  • 匿名
2013-05-23 12:28:18
我们在互相颗粒的腐蚀状态,机械测试上为化学结构测试不锈钢管子。很遗憾,在到互相颗粒的腐蚀状态的钢铁铅中的钛的缺席,到使钢过热的倾向。在这样的烟斗的炫耀期间不是钢的足够坚韧,它不允许在 tubesheet 方面紧密制作烟斗的炫耀。压力被应用到设备时可以导致化合物的撤销加压。
 
 