求翻译:3. In a tensile test, the a 0-martensite formation starts at low true strains before 5% and the highest rate of transformation occurs at true strains of 20%. The slow transformation and the fact that the fraction of strain-induced a 0-martensite remains quite low, reaching 40%, are beneficial factors to attain a very是什么意思?

待解决 悬赏分:1 - 离问题结束还有
3. In a tensile test, the a 0-martensite formation starts at low true strains before 5% and the highest rate of transformation occurs at true strains of 20%. The slow transformation and the fact that the fraction of strain-induced a 0-martensite remains quite low, reaching 40%, are beneficial factors to attain a very
问题补充:

  • 匿名
2013-05-23 12:21:38
3.在拉伸试验中,一个0马氏体的形成开始于低真应变前5 %和转化率最高发生在? 20 %,真正的压力。
  • 匿名
2013-05-23 12:23:18
正在翻译,请等待...
  • 匿名
2013-05-23 12:24:58
3. 在一个拉伸测试, 0马氏体形成在5%之前以低真实的张力开始,并且变革的最高的速率发生在真实的张力 20%。 缓慢的变革和事实分数张力导致0马氏体遗骸的相当低,到达 40%,是获得非常高一致的伸长的有利因素
  • 匿名
2013-05-23 12:26:38
3.在拉伸试验中,0 马氏体的形成始于低 5%之前的真实菌株和最高的转换率发生在真实菌株的 20%。缓慢的变革和事实的分数应变诱发马氏体 0 仍然相当低,达到了 40%,是要达到非常高的均匀伸长率的有利因素
  • 匿名
2013-05-23 12:28:18
3.In a tensile test, the a 0-martensite formation starts at low true strains before 5% and the highest rate of transformation occurs at true strains of 20%.The slow transformation and the fact that the fraction of strain-induced a 0-martensite remains quite low, reaching 40%, are beneficial factor
 
 