当前位置:首页 » 翻译 
  • 匿名
关注:1 2013-05-23 12:21

求翻译:144h试验后金属件边缘及棱角部位2mm以外的镀层不应有锈点。是什么意思?

待解决 悬赏分:1 - 离问题结束还有
144h试验后金属件边缘及棱角部位2mm以外的镀层不应有锈点。
问题补充:

  • 匿名
2013-05-23 12:21:38
144h after the test pieces of metal coating other than edge and corner position 2mm there should be no rust.
  • 匿名
2013-05-23 12:23:18
After 144 H test edge metal parts and corners parts other than the 2mm coated undue rust.
  • 匿名
2013-05-23 12:24:58
After the 144h experiment the metal edge and outside the edges and corners spot 2mm coating should not have the rust spot.
  • 匿名
2013-05-23 12:26:38
144h after the test pieces of metal coating other than edge and corner position 2mm there should be no rust.
  • 匿名
2013-05-23 12:28:18
144h after the test pieces of metal coating other than edge and corner position 2mm there should be no rust.
 
 