求翻译:The stress corrosion of 304L and 316L stainless steels has been studied in MgCl2 44 % at 153°C. Stress corrosion tests are carried out under constant load and galvanostatic control at i = 0 in order to be near free corrosion potential conditions. During the tests, the sample elongation, the electrode potential, the mod是什么意思? 待解决
悬赏分:1
- 离问题结束还有
The stress corrosion of 304L and 316L stainless steels has been studied in MgCl2 44 % at 153°C. Stress corrosion tests are carried out under constant load and galvanostatic control at i = 0 in order to be near free corrosion potential conditions. During the tests, the sample elongation, the electrode potential, the mod
问题补充: |
|
2013-05-23 12:21:38
304L和316L不锈钢应力腐蚀已经研究了氯化镁44%,在153 ° C。 I = 0时以接近免费腐蚀电位条件下进行应力腐蚀试验恒定负载和恒电流控制。在测试过程中,样品伸长,电极电位,模量和阶段的阻抗随时间变化的记录。在SCC的钝化膜的电化学行为现象进行了研究。同样的演变是观察的潜力和阻抗模,但会出现一个阶段的最大尽快潜在的展品在其anodical值增加一个拐点。 SEM观察表明,最大相对应的裂纹扩展开始。电化学阻抗技术,似乎更具吸引力遵循的钝化膜的演变,直到然后用更精确检测的裂纹扩展比样品伸长年初。
|
|
2013-05-23 12:23:18
在强调腐蚀的不锈钢304L和316L在MgCl2已经研究了钢材44%在153°C 强调腐蚀试验是在不断进行负载和galvanostatic控制在I=0,以便将靠近免费腐蚀可能条件。 在进行测试,样本的延伸率,在电极潜力,
|
|
2013-05-23 12:24:58
|
|
2013-05-23 12:26:38
|
|
2013-05-23 12:28:18
|
湖北省互联网违法和不良信息举报平台 | 网上有害信息举报专区 | 电信诈骗举报专区 | 涉历史虚无主义有害信息举报专区 | 涉企侵权举报专区