求翻译:Annealing at 500 C for 1 h leads to enhanced L12 ordering in FeCoCr(Ni)-rich domains, but no obvious microstructure coarsening can be seen, suggesting that the alloy with two coherent fcc nanophases has a high thermal stability for potential applications at high temperatures.是什么意思?

待解决 悬赏分:1 - 离问题结束还有
Annealing at 500 C for 1 h leads to enhanced L12 ordering in FeCoCr(Ni)-rich domains, but no obvious microstructure coarsening can be seen, suggesting that the alloy with two coherent fcc nanophases has a high thermal stability for potential applications at high temperatures.
问题补充:

  • 匿名
2013-05-23 12:21:38
退火,在500 2 C 1小时导致FeCoCr (Ni)的增强L12订货富含结构域,但没有明显的显微组织粗化可以看出,这表明有两个相干的fcc nanophases该合金具有高的潜在应用高的热稳定性
  • 匿名
2013-05-23 12:23:18
正在翻译,请等待...
  • 匿名
2013-05-23 12:24:58
焖火在500  C为1 h导致改进的L12命令在FeCoCr( Ni) -富有的领域,但明显的微结构变粗不能看,建议合金与二连贯fcc nanophases有高耐热性为潜在的应用在高温。
  • 匿名
2013-05-23 12:26:38
1 小时 500 ℃ 退火导致增强 L12 订购的 FeCoCr (Ni)-丰富的域,但没有明显的显微组织粗化中可以看出,表明与两个相干的 fcc 纳米相合金在高温下有较高的热稳定性,为潜在的应用。
  • 匿名
2013-05-23 12:28:18
Annealing at 500 C for 1 h leads to enhanced L12 ordering in FeCoCr(Ni)-rich domains, but no obvious microstructure coarsening can be seen, suggesting that the alloy with two coherent fcc nanophases has a high thermal stability for potential applications at high temperatures.
 
 