求翻译:Electrochemical noise (EN) analyses, using time domain, frequency domain and statistical parameters, were carried out on the potential and current data obtained on AISI type 316 stainless steel during (i) pitting corrosion in deaerated 0.5 M sodium chloride (NaCl) solution, and during (ii) stress corrosion cracking (SC是什么意思?

待解决 悬赏分:1 - 离问题结束还有
Electrochemical noise (EN) analyses, using time domain, frequency domain and statistical parameters, were carried out on the potential and current data obtained on AISI type 316 stainless steel during (i) pitting corrosion in deaerated 0.5 M sodium chloride (NaCl) solution, and during (ii) stress corrosion cracking (SC
问题补充:

  • 匿名
2013-05-23 12:21:38
电化学噪声(EN)分析,使用时域,频域和统计参数,进行了对AISI 316不锈钢在(I)点蚀腐蚀除氧0.5 M的氯化钠(盐)解决方案获得的潜在的和现有的数据,期间(二)在沸腾的酸性NaCl溶液中的应力腐蚀开裂(SCC)。视觉纪录,以及现有的和潜在的数据统计分析,使用最大熵法(MEM)给谱估计alongwith区分这些腐蚀过程和有用的信息上的压力在加速点蚀的效果。相关的结果,以及与光学显微镜观察。
  • 匿名
2013-05-23 12:23:18
电化学噪音(EN)分析,使用时域、频率域和统计参数,进行的潜力和目前关于非洲信息社会倡议取得的数据类型316不锈钢在(i)对立的腐蚀deaerated0.5m氯化钠(以NaCL)解决方案,和在(ii)强调腐蚀性裂缝(SCC)以滚酸化氯化钠NaCl解决。
  • 匿名
2013-05-23 12:24:58
  • 匿名
2013-05-23 12:26:38
电化学噪声 (EN) 分析,使用时间域,频率域和统计参数,进行 AISI 类型 316 不锈钢在 (i) 除氧的 0.5 米 (氯化钠) 氯化钠溶液,点蚀和 (ii) 应力腐蚀开裂 (SCC) 沸腾酸化的氯化钠溶液中期间获得的潜在的和当前数据%